35H360 Non Grain Oriented Electrical steel
Low iron loss is one important feature of 35H270 Non Grain Oriented Electrical steel. This means that it is able to maintain a strong magnetic field without losing energy to heat, making it ideal for use in transformers, reactors, and other electrical devices where efficiency is critical.

35H360 Steel Specifications
| Thickness | Assumed Density |
Core Loss(W/Kg) | Core Loss(W/Lb) | Induction (800A/m) |
Lamination Factor (Minimum) |
Remark | ||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 50Hz | 60Hz | 50Hz | 60Hz | |||||||||
| mm | Kg/dm3 | 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | |||
| 0.35 | 7.65 | 1.45 | 3.60 | 1.85 | 4.55 | 0.66 | 1.63 | 0.84 | 2.06 | 1.63 | 95.0 | - |
35H360 silicon Steel Typical Electrical and Magnetic Properties
| Assumed Density |
Resistivity | Core Loss | Induction T |
||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| W/Kg | W/LB | ||||||||||
| Kg/dm3 | Ohm*Meter (X10e-8) |
50Hz | 60Hz | 50Hz | 60Hz | ||||||
| 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | 1.0T | 1.5T | 2,500A/m | 5,000A/m | ||
| 7.65 | 45 | 1.26 | 2.80 | 1.56 | 3.48 | 0.57 | 1.27 | 0.71 | 1.58 | 1.59 | 1.68 |
35H360 Electrical Steel Typical Mechanical Properties and Lamination Factors
| Tensiile Strength | Yield Point | Elongation % |
Hardness Hv(1) |
Bending Test Value |
Lamination Factor % |
||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| N/mm2 | lb/in2(X10e3) | N/mm2 | lb/in2(X10e3) | ||||||||||
| L | C | L | C | L | C | L | C | L | C | L | C | ||
| 471 | 481 | 68 | 70 | 333 | 343 | 48 | 50 | 29 | 30 | 164 | 31 | 27 | 98.0 |
Populární Tagy: 35h360 non grain oriented electrical steel, China, suppliers, manufacturers, factory, buy, price, pricelist, for sale, in stock, free sample